Show simple item record

dc.contributor.authorMneimne, Men_US
dc.contributor.authorHill, RGen_US
dc.contributor.authorBushby, AJen_US
dc.contributor.authorBrauer, DSen_US
dc.date.accessioned2011-05-31T09:49:44Z
dc.date.available2010-11-23en_US
dc.date.issued2011-04en_US
dc.identifier.issn1742-7061en_US
dc.identifier.urihttp://qmro.qmul.ac.uk/xmlui/handle/123456789/1101
dc.descriptionNOTICE: this is the author’s version of a work that was accepted for publication in Acta Biomaterialia. Changes resulting from the publishing process, such as peer review, editing, corrections, structural formatting, and other quality control mechanisms may not be reflected in this document. Changes may have been made to this work since it was submitted for publication. A definitive version was subsequently published in Acta Biomaterialia, [VOL 7, ISSUE 4, (2001)] DOI: 10.1016/j.actbio.2010.11.037en_US
dc.format.extent1827 - 1834en_US
dc.relation.ispartofACTA BIOMATERen_US
dc.subjectDentifricesen_US
dc.subjectToothpasteen_US
dc.subjectFluorideen_US
dc.subjectBioactive glassen_US
dc.subjectFluorapatiteen_US
dc.subjectLIME-PHOSPHOSILICATE GLASSESen_US
dc.subjectSIMULATED BODY-FLUIDen_US
dc.subjectDEGRADATIONen_US
dc.subjectDENTIFRICEen_US
dc.subjectBEHAVIORen_US
dc.subjectNMRen_US
dc.titleHigh phosphate content significantly increases apatite formation of fluoride-containing bioactive glassesen_US
dc.typeArticle
dc.identifier.doi10.1016/j.actbio.2010.11.037en_US
pubs.issue4en_US
pubs.notesNot knownen_US
pubs.volume7en_US


Files in this item

Thumbnail

This item appears in the following Collection(s)

Show simple item record